Adding Sn, Ni, and other trace elements to copper as the matrix gives it high strength, elasticity, and excellent stress relaxation performance. Commonly used for lead frames, automotive terminals, connectors, etc.
Grade
Chemical composition(%)≤
Thickness
(mm)
ASTM
Cu
Sn
Ni
P
Zn
Other
0.1-3.0
C19040
Balance
1.0-2.0
0.7-0.9
0.02-0.09
0.01-0.3
≤1.0
Physical properties
Density
(g/cm³)
Modulus of elasticity
(GPa)
Thermal expansion coefficient
(×10-6/K)
Electrical conductivity
(%IACS)
Thermal conductivity
W(m·K)
8.9
130
17
30
140
Mechanical properties
Bend properties
Temper
Hardness
HV
Tension test
90°R/T(Thick<0.8mm)
Tensile Strength
Rm/MPa
Yield Strength
MPa
Elongation
%
Good way
Bad way
H04
155-180
500-590
480-565
≥8
0
0.5
H06
160-195
540-630
525-610
≥6
0.5
1
FAQ
Q: How long is your delivery time?
A: Generally it is within 15 days if the goods are in stock. or it is less than 30 days if the goods are not in stock, it is according to quantity.
Q: Do you provide samples ?
A: Yes, we could offer the sample
Q: What ls your terms of payment
A.30% T/T in advance ,balance before shipment. And the price depends on the material and the quantity
If you have another question, please feel free to contact us.